A higher standard.
Theres nothing ordinary about Trumbull standard built-up roofing asphalts. Like every asphalt we make, our standard Types I - IV asphalts meet or exceed ASTM standards in every category.
We exceed ASTM minimum softening points to minimize the risk of slippage and reduce "fallback." We use high flashpoint raw materials to provide added safety. We also widen the spread between equiviscous temperature (EVT) and flashpoint to support application, adhesion and waterproofing.
And to make sure our products are consistently reaching those standards, we test not once, but twice. First theyre tested at our on-site plant laboratories then again at our Summit, Illinois, Technological Laboratory one of a select few certified by the AASHTO (American Association of State Highway Testing Officials.)
Enhancing the capabilities of asphalt to better address your needs. We call it Applied Innovation. You know it as Trumbull quality. The highest standard in the built-up roofing asphalt industry.
Standard Type I - IV Asphalts MSDS Sheet
|
| Features |
Benefits |
| All products meet ASTM D312 |
Each shipment meets or exceeds the physical requirements of the specified roofing grade asphalt |
|
| Consistent high flash material |
Proper temperature range needed to apply product safely at the EVT; flash points typically 50ºF to 75ºF higher than the 500ºF minimum |
|
| Testing in each plant and at Summit, IL laboratory |
All Owens Corning Trumbull products are assured to meet ASTM requirements |
|
| 19 producing plants |
Convenient, accessible availability from coast to coast |
|
| EVT shown on each carton and bill of lading for bulk shipments |
Assures proper adhesion, waterproofing and application rate |
|
| Printed cartons |
Clearly identifies manufacturers, type, flash point, EVT, production location and production date |
Physical Requirements - ASTM D312-00
| |
Type I |
Type II |
Type III |
Type IV |
Test Methods |
| |
Min. |
Max. |
Min. |
Max. |
Min. |
Max. |
Min. |
Max. |
| Softening Point (ºF) |
135 |
151 |
158 |
176 |
185 |
205 |
210 |
225 |
ASTM D36 |
|
| Flash Point (ºF) |
500 |
|
500 |
|
500 |
|
500 |
|
ASTM D92 |
|
| Penetration, Units, dmm: |
| @32ºF |
3 |
|
6 |
|
6 |
|
6 |
|
ASTM D5 |
| @77ºF |
18 |
60 |
18 |
40 |
15 |
35 |
12 |
25 |
|
| @115ºF |
90 |
180 |
|
100 |
|
90 |
|
75 |
|
|
| Ductility @77ºF, cm |
10.0 |
|
3.0 |
|
2.5 |
|
1.5 |
|
ASTM D113 |
|
| Solubility in Trichoroethylene % |
99 |
|
99 |
|
99 |
|
99 |
|
ASTM D2042 |
|
| Asphalts shall be homogenous and free of water and shall conform to these physical properties |
Typical Physical Characteristics for Trumbull Asphalt
| |
Type I |
Type II |
Type III |
Type IV |
|
| Softening Point (ºF) |
140-145 |
165-175 |
195-205 |
210-225 |
|
|
| Flash Point (ºF) |
525 |
525 |
525 |
525 |
|
|
| Penetration, Units, dmm: |
| @32ºF |
6 |
8 |
6 |
6 |
|
| @77ºF |
20-35 |
18-30 |
16-24 |
13-22 |
|
|
| Ductility @77ºF, cm |
13 |
4.0 |
3.0 |
2.0 |
|
|
| Solubility in Trichoroethylene % |
99.8 |
99.8 |
99.8 |
99.8 |
|
|
| Typical Application Temperature |
|
|
|
|
|
| For Hand Mopping |
|
|
|
|
|
| EVT @125 CPS +/- 25ºF |
350 |
375 |
410 |
440 |
|
| For Machine Spreader |
|
|
|
|
|
| EVT @ 75 CPS +/- 25ºF |
370 |
395 |
430 |
460 |
|
|
| Plant Specific EVTs |
|