RhinoMat®

Owens Corning RhinoMat 1000 Reinforced Composite Geomembrane is an engineered geosynthetic liner designed for superior performance in water containment and retention applications.

Download Brochure PDF | 907KB

Owens Corning RhinoMat 1000 Reinforced Composite Geomembrane is an engineered geosynthetic liner designed for superior performance in water containment and retention applications.

Download Brochure PDF | 907KB

Specifications and Literature

Product Features

2X Puncture Resistance

Reduce punctures and leaks with Owens Corning RhinoMat Reinforced Composite Geomembranes (RCG). With double the puncture resistance of standard 60mil HDPE*, RhinoMat RCG is engineered to minimize punctures and leaks.

Strong UV Stability

UV-resistant, highly flexible and lightweight construction of RhinoMat RCG provides maximum performance in many different climates and environmental conditions.

Easy to Handle

The highly flexible and lightweight construction of RhinoMat RCG helps make it easier to handle and install than conventional HDPE.

Resources

Technical Information

The [ 30 ] mil RCG shall have the following properties:

Property

Test Method

Typical Value

Marv

Weight

ASTM D5261

18 oz./yd2

17.1 oz./yd2

Thickness

ASTM D751

33.5 mil

30 mil

Strip Tensile Strength (MD)

ASTM D7003

246 lbf

224 lbf

Strip Tensile Strength (CD)

ASTM D7003

272 lbf

262 lbf

Strip Tensile Elongation (MD)

ASTM D7003

21%

20%

Strip Tensile Elongation (CD)

ASTM D7003

22%

20%

Tongue Tear (MD)

ASTM D5884

56 lbf

50 lbf

Tongue Tear (CD)

ASTM D5884

56 lbf

50 lbf

CBR Puncture

ASTM D6241

1348 lbf

1301 lbf

Index Puncture Resistance

ASTM D4833

230 lbf

199 lbf

Hydrostatic Resistance

ASTM D751

729 lb/in2

705 lb/in2

Dimensional Stability3

ASTM D1204

1.52%

N/A

Water Vapor Transmission3

ASTM E96

0.09 g/m2-day

N/A

UV Resistance (Fluorescent Light Method)4

ASTM D7238

a) Strength & Elongation retained after 10,000 light hours

ASTM D7003

> 90% retained

> 90% retained

b) Response to bending

GRI GM-16

no cracking

no cracking

Grab Tensile Strength (MD)

ASTM D751

385 lbf

N/A

Grab Tensile Strength (CD)

ASTM D751

385 lbf

N/A%

Trapezoidal Tear (MD)

ASTM D4533

66 lbf

N/A

Trapezoidal Tear (CD)

ASTM D4533

66 lbf

N/A

Seam Strength (Shear)5

ASTM D7747

100 lbf

N/A

Seam Strength (Peel)6

ASTM D7747

25 lbf

N/A

Hydraulic Conductivity

ASTM E96 (‘B’)

1.0 x 10-14 cm/sec

20%

Carbon Black Content

ASTM D4218

> 2%

N/A

Accelerated UV Weathering7

ASTM G154

> 90% @ 10,000 hrs.

N/A

Low Temperature Brittleness

ASTM D2136

Pass (@ -60°F)

N/A

The [ 40 ] mil RCG shall have the following properties:

Property

Test Method

Typical Value

Marv

Weight

ASTM D5261

20.8 oz./yd2

20.3 oz./yd2

Thickness

ASTM D751

40 mil

36 mil

Strip Tensile Strength (MD)

ASTM D7003

303 lbf

285 lbf

Strip Tensile Strength (CD)

ASTM D7003

265 lbf

259 lbf

Strip Tensile Elongation (MD)

ASTM D70003

22%

20%

Strip Tensile Elongation (CD)

ASTM D7003

22%

20%

Tongue Tear (MD)

ASTM D5884

60 lbf

50 lbf

Tongue Tear (CD)

ASTM D5884

62 lbf

50 lbf

CBR Puncture

ASTM D6241

1400 lbf

1360 lbf

Index Puncture Resistance

ASTM D4833

242 lbf

220 lbf

Hydrostatic Resistance

ASTM D751

740 lb/in2

707 lb/in2

Dimensional Stability3

ASTM D1204

2.86%

N/A

Water Vapor Transmission3

ASTM E96

0.08 g/m2-day

N/A

UV Resistance (Fluorescent Light Method)4

ASTM D7238

a) Strength & Elongation retained after 10,000 light hours

ASTM D7003

> 90% retained

> 90% retained

b) Response to bending

GRI GM-16

no cracking

no cracking

Grab Tensile Strength (MD)

ASTM D751

463 lbf

N/A

Grab Tensile Strength (CD)

ASTM D751

397 lbf

N/A

Trapezoidal Tear (MD)

ASTM D4533

73 lbf

N/A

Trapezoidal Tear (CD)

ASTM D4533

69 lbf

N/A

Seam Strength (Shear)5

ASTM D7747

165 lbf

N/A

Seam Strength (Peel)6

ASTM D7747

30 lbf

N/A

Hydraulic Conductivity

ASTM E96 (‘B’)

1.0 x 10-14 cm/sec

N/A

Carbon Black Content

ASTM D4218

> 2%

N/A

Accelerated UV Weathering7

ASTM G154

> 90% @ 10,000 hrs.

N/A

Low Temperature Brittleness

ASTM D2136

Pass (@ -60°F)

N/A

  1. Typical values represent an average test result for the sample size, with + 10% variance
  2. Minimum Average Roll Values (MARV) are shown (unless otherwise noted), in accordance with GRI-GM30
  3. Dimensional Stability and Water Vapor Transmission values shown are maximum test result values
  4. Test samples were exposed to UV radiation using this method prior to evaluating changes in material properties
  5. Test values reflect single-track wedge welding at approximately 750° F and 14 ft/sec
  6. Test values reflect single-track wedge welding at approximately 750° F and 14 ft/sec
  7. Test valued based on A-340 lamps, 8 hours UV @ 60° C, 4 hours condensation @ 40° C